Compositio chemica
| Standard | Gradus | C | Mn | P | S | Si | Ni | Cr | Mo |
EN 10084 |
18CrNiMo7-6 | 0.15-0.21 |
0.50-0.90 |
≤ 0.025 |
≤ 0.035 |
≤ 0.04 |
1.4-1.7 |
1.5-1.8 |
0.25-0.35 |
| 1.6587 |
Corporalis Property
| Densitas, g/cm3 | 7.85 | ||||
| Imprimis caloris capacitas J/(kg.K) | 460 | ||||
| Electric resistivity Ohm.mm2 /m | 0.18 | ||||
| Electric conductivity Siemens.m/mm2 | 5.55 | ||||
| Modulus elasticitatis Gpa | 210 | ||||
| Scelerisque expansio 10^6 m/(m.K) | 100 ℃ | 200 ℃ | 300 ℃ | 400 ℃ | 500 ℃ |
| 11.1 | 12.1 | 12.9 | 13.5 | 13.9 | |
Mechanica Property
| Magnitudo mm | ≤ 11 | 12-30 | 31-63 |
| R Mpa | 1180-1420 | 1080-1320 | 980-1270 |
| Rp 0.2 Mpa | ≥ 835 | ≥785 | ≥ 685 |
| A % | ≥ 7 | ≥ 8 | ≥ 5 |
| C % | ≥ 30 | ≥ 35 | ≥ 35 |
| Kv J | ≥ 44 | ≥ 44 | |
| duritia HB | 354-406 | 327-384 | 295-373 |
Forging
DIN 1.6587 | 17CrNiMo6 |18CrNiMo7-6 calfaciendi temperies: 900 - 1100°C, lente in arena frigido postquam ementiebatur.
Calor treatment
Superficies duritia
Applicationem
DIN 1.6587 | 17CrNiMo6 |18CrNiMo7-6 ferrum ad partes, quae nucleum vim distrahentes et altitudinem duritiem requirunt. Susceptibilis ad partes magnas occupatas cum magna resistentia et onerantium ut: Gravis Officium Bushings et Partes, Cam Sectatores, Canes Clutch, Compressor Repagula, Extractors, Fan Shafts, Gravis Officium Gears, Pump Shafts, Sprockets, Tappets, Gerunt acus, Filum Duces elc.
Q: Quid nobiscum eligite?
A: habemus professionales team, servitium et inspectionem.
Q: Quam longum est tempus tuum traditio?
A: generaliter est 5-10 dies in sunt in struncum.
Vel est 15-20 dies si bona nostra in stirpe, pro quantitatem.
Q: Videte exempla ? Estne liberum vel extra ?
A: potuimus exemplum Exemplum gratis potuimus exemplum Exemplum pro gratis offerre potuimus.
Q: Quam est te in tuo nostra protooli?
A: Pretio<=1000USD, 100% in promotionem. Mercedem>=1000USD, 30% T/T in promove, balsamum ante navigationem.
Si tuam aliam quaestionem habes, pis fac libera nos in contactum.