Mga produkto
We have professional sales team numbered 200 with more than 16 years experience.
Posisyon:
Bahay > Mga produkto > Steel Plate > Steel Plate sa paggawa ng mga barko
CCS Shipbuilding steel plate
CCS Shipbuilding Plate
CCS Shipbuilding Plate
CCS Shipbuilding Plate

CCS shipbuilding steel plate

CCS shipbuilding plate grade AQ DQ EQ FQ AH EH FH 36 40 47 51 63 70 kemikal at mekanikal na katangian
Panimula ng produkto
CCS Shipbuilding Plate

CCS Grade FQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
690 770-940 14

CCS Grade EQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
690 770-940 14

CCS Grade DQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.035 0.035 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
690 770-940 14--16

CCS Grade AQ70 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
690 770-940 14

CCS Grade EQ63 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
620 720-890 15

CCS Grade FQ63 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
620 720-890 15

CCS Grade AQ63 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
620 720-890 15

CCS Grade EQ56 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
550 670-830 16

CCS Grade FQ56 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
550 670-830 16

CCS Grade AQ56 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.60 0.030 0.030 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
550 670-830 16

CCS Grade EQ51 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
500 610-770 16

CCS Grade FQ51 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
500 610-770 16

CCS Grade AQ51 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
500 610-770 16

CCS Grade EQ47 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.20 0.55 1.70 0.025 0.025 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
460 570-720 17

CCS Grade FQ47 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.18 0.55 1.60 0.020 0.020 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
460 570-720 17

CCS Grade AQ47 Shipbuilding Steel Plate

C max Si max Mn P max S max N max.
0.21 0.55 1.70 0.030 0.030 0.020
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
460 570-720 17
Teknikal na data

CCS Grade EH40 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.18 0.50 0.90-1.60 0.025 0.025 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
390 510-660 20

CCS Grade FH40 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.16 0.50 0.90-1.60 0.020 0.020 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.80 0.08 0.009
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
390 510-660 20

CCS Grade AH40 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.18 0.50 0.90-1.60 0.030 0.030 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
390 510-660 20

CCS Grade EH36 Shipbuilding Steel Plate

C max Si max Mn P max S max Als Nb V Ti max. Cu max. Cr max. Ni max. Mo max. N max.
0.18 0.50 0.90-1.60 0.025 0.025 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Lakas ng Yield (MPa) min. Lakas ng Tensile (MPa) Pagpahaba min. %
355 490-630 21

CCS/E Normal Strength Max Chemical Composition sa Hot-rolled

Elemento CCS E Max % Elemento CCS E Max %
C 0.21 Ni
Mn 0.60 Mo
Si 0.1-0.35 Sinabi ni Al
S 0.035 Nb
P 0.035 V
Cu Ti
Cr N
Sensitivity ng Crack: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas ng Carbon: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
CCS/E Normal strength property sa Hot-rolled
Grade kapal Lakas ng Yield Lakas ng makunat Pagpahaba Enerhiya ng Epekto
(mm) MPa (min) MPa % (min) (KV J) (min)
-20 degree
CCS E 8-240 235 400-520 22 27J

Tandaan: ang epekto ng enerhiya sa ilalim ng mas mababa sa 50mm kapal; longitudinal min impact energy

CCS/D Normal Strength Max Chemical Composition sa Hot-rolled

Elemento CCS D  Max % Elemento CCS D  Max %
C 0.21 Ni
Mn 0.60 Mo
Si 0.1-0.35 Sinabi ni Al
S 0.035 Nb
P 0.035 V
Cu Ti
Cr N
Sensitivity ng Crack:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas ng Carbon:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

CCS/D Normal strength property sa Hot-rolled

Grade kapal Lakas ng Yield Lakas ng makunat Pagpahaba Enerhiya ng Epekto
(mm) MPa (min) MPa % (min) (KV J) (min)
-20 degree
CCS D 8-240 235 400-520 22 27J

Tandaan: ang epekto ng enerhiya sa ilalim ng mas mababa sa 50mm kapal; longitudinal min impact energy

CCS/B Normal Strength Max Chemical Composition sa Hot-rolled

Elemento CCS B  Max % Elemento CCS B  Max %
C 0.21 Ni
Mn 0.80 Mo
Si 0.35 Sinabi ni Al
S 0.035 Nb
P 0.035 V
Cu Ti
Cr N
Sensitivity ng Crack:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas ng Carbon:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

CCS/B Normal strength property sa Hot-rolled

Grade kapal Lakas ng Yield Lakas ng makunat Pagpahaba Enerhiya ng Epekto
(mm) MPa (min) MPa % (min) (KV J) (min)
0 degree
CCS B 8-240 235 400-520 22 27J

Tandaan: ang epekto ng enerhiya sa ilalim ng mas mababa sa 50mm kapal; longitudinal min impact energy

CCS/A Normal Strength Max Chemical Composition sa Hot-rolled

Elemento CCS A Max % Elemento CCS A Max %
C 0.21 Ni
Mn 2.5*C MIN Mo
Si 0.50 Sinabi ni Al
S 0.035 Nb
P 0.035 V
Cu Ti
Cr N

Sensitivity ng Crack:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+ 5B)%
Katumbas ng Carbon:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

CCS/A Normal strength property sa Hot-rolled

Grade kapal Lakas ng Yield Lakas ng makunat Pagpahaba Enerhiya ng Epekto
(mm) MPa (min) MPa % (min) (KV J) (min)
20 degree
CCS A 8-240 235 400-520 22
Tandaan: ang epekto ng enerhiya sa ilalim ng mas mababa sa 50mm kapal; longitudinal min impact energy

Kaugnay na Mga Produkto
CCS AH36 DH36 EH36 FH36 Marine Steel Plate
CCS FH36 Marine Steel Plate
CCS EH36 Marine Steel Plate
CCS AH36 Marine Steel Plate
ASTM A131 Grade A/B Marine Steel plate
ABS Grade AH32 Shipbuilding Steel plate
ABS Grade EH32 Shipbuilding Steel Plate
LR Grade EH40 Marine Steel Plate
CCS AH40 DH40 EH40 FH40 Marine Steel Plate
CCS FH40 Marine Steel Plate
CCS EH40 Marine Steel Plate
CCS DH40 Marine Steel Plate
CCS AH40 Marine Steel Plate
RINA Grade AH40 DH40 EH40 FH40 Marine Steel Plate
RINA Grade FH40 Marine Steel Plate
RINA Grade EH40 Marine Steel Plate
RINA Grade DH40 Marine Steel Plate
RINA Grade AH40 Marine Steel Plate
RINA Grade AH36 DH36 EH36 FH36 Marine Steel Plate
RINA Grade FH36 Marine Steel Plate
RINA Grade EH36 Marine Steel Plate
RINA Grade AH36 Marine Steel Plate
B480GNQR Bakal
RINA Grade AH32 DH32 EH32 FH32 Marine Steel Plate
RINA Grade FH32 Marine Steel Plate
RINA Grade EH32 Marine Steel Plate
Pagtatanong
* Pangalan
* E-mail
Telepono
Bansa
Mensahe